Availability: | |
---|---|
Ceramic sand isa specialized type of sand used in foundry applications, known for its high refractoriness, spherical shape, and low thermal expansion. It's a manufactured product, often made from fused bauxite, and offers several advantages over traditional silica sand in casting processes.
NO. | ITEM | RESULT |
1 | Al2O3 | 70.30% |
2 | Fe2O3 | 1.98% |
3 | Coefficient of Angularity | 1.06 |
4 | Pelletizing Rate | 99% |
5 | Bulk Specific Weight | 1.95-2.05g/cm3 |
6 | Refractoriness | >1790ºC |
7 | Thermal Conductivity | (1200ºC)5.27W/M.K |
8 | PH | 7-8 |
PARTICLE DISTRIBUT | ||
1 | 30 MESH | 6.5 |
2 | 40 MESH | 36.8 |
3 | 50 MESH | 40.1 |
4 | 70 MESH | 13.9 |
5 | 100 MESH | 2.5 |
6 | 140 MESH | 0.2 |
7 | AFS | 37.2 |
Application
Widely used in foundry technique like resinbonded sand, sodium silicate sand, and clay-bonded sand for sand core and casting mould making
Replace chromite sand and widely used in sand core making like jacket core, oil duct core, tappet core of engine
Replace chromite sand for steel casting facing sand and sub-layer of molding sand (backing sand)
Widely used as dry sand and sand box for EPC process and V method of casting processes
Widely used as the main raw materials of advanced refractory products (Ladle drainage sand,gravity casting material, casting coating, etc.)
Widely used as cleaning sand for copper and aluminum alloy castings
Characteristic
1. The melting point is over 1800℃.
2. It has good fluidity and a low edge angle coefficient.
3. It is suitable for the appropriate particle size distribution of most casting techniques.
4. Low humidity.
5. Low thermal expansion rate.
6. Good thermal conductivity and good air permeability.
7. High bending strength and pressing strength.
Applications in foundries:
No-Bake Processes:Improves sand strength, reduces binder levels, and increases reclamation yields.
Resin Coated Sand (RCS) Cores:Enhances flowability, reduces expansion and gas evolution.
Sodium Silicate Systems:Reduces binder consumption, enhances shake-out properties, and minimizes defects like penetration and sand burn-on.
Lost Foam Casting:Improves flowability, filling, and permeability.